Portland Cement: Raw Materials, the Rotary Kiln and How Cement Sets

Sstem notes·Aperturebiolabs·Edited 4 weeks ago·4 min read
Calcium CationCarbonate IonCarbon DioxideOxidecement-manufacturingchemical-hydrationconstruction-technologyindustrial-chemistrymaterials-science

Cement is the binder in concrete and mortar, the most widely used construction material on Earth. The modern type, Portland cement, was patented by Joseph Aspdin in 1824, who named it after the pale Portland building stone it resembled once set. It is made by strongly heating an intimate mixture of a lime-rich (calcareous) material and a clay-rich (argillaceous) material until they partly fuse into clinker, which is then ground to a fine powder with a little gypsum.

Raw Materials and Composition

Calcareous materials such as limestone, chalk, marble and marine shells supply calcium oxide. Argillaceous materials such as clay, shale and blast-furnace slag supply the acidic oxides silica and alumina, plus some iron oxide. Gypsum is added at the end. A typical Portland cement contains:

Typical composition of Portland cement (as oxides)

Oxide

CaO

SiO₂

Al₂O₃

Fe₂O₃

MgO

SO₃

Na₂O + K₂O

Mass %

60–67

20–23

4–8

2–4

1–3

1.5–3

about 1

Making Cement

The raw materials are crushed and ground together, in roughly 3 : 1 proportions of limestone to clay. In the wet process, grinding is done with water to give a slurry of 35–45% water. This makes mixing easy and dust-free, but evaporating all that water costs a lot of fuel. The dry process grinds the materials dry; with modern cyclone preheaters it uses far less energy, and it is now the usual choice. Either way, the mix is fed into the upper end of a rotary kiln: a long steel cylinder lined with firebrick, slightly tilted and slowly turning, with a flame of coal, oil or gas at the lower end. As the charge tumbles down through hotter and hotter zones over a few hours, it changes in stages:

  1. Drying zone, up to about 500 °C: water is driven off, and the clay breaks down into silica, alumina and iron oxide.
  2. Decomposition (calcining) zone, about 900 °C: limestone loses carbon dioxide and becomes lime.
  3. Burning (clinkering) zone, about 1400–1500 °C: lime reacts with the other oxides, and partial melting forms the clinker minerals.
  4. Cooling zone: the grey-green clinker nodules, from nut to pea size, cool before leaving the kiln.

Calcining limestone in the kiln (about 900 °C; the major source of CO2 from cement)
[Ca+2].[O-]C([O-])=O>>[Ca+2].[O-2].O=C=O

The main clinker minerals

Mineral

Formula (oxide notation)

Role

Tricalcium silicate (alite)

3CaO·SiO₂

Early strength (first weeks)

Dicalcium silicate (belite)

2CaO·SiO₂

Slow, long-term strength

Tricalcium aluminate

3CaO·Al₂O₃

Reacts very fast; causes flash set

Tetracalcium aluminoferrite

4CaO·Al₂O₃·Fe₂O₃

Gives grey colour; acts as a flux

The cooled clinker is ground to a very fine powder with about 2–5% gypsum. Calcining limestone and burning fuel make cement production responsible for roughly 8% of global \mathrm{CO_2} emissions, which is why the industry is developing lower-carbon cements.

How Cement Sets

Cement does not set by drying. It sets by hydration, reacting with water to form new, interlocking solids, so concrete hardens even under water. Within minutes, tricalcium aluminate reacts with water. On its own this would set the paste solid almost at once (flash set), but gypsum reacts with it to form needle-like crystals of calcium sulphoaluminate (ettringite) that coat the grains and slow the reaction, giving time to place the concrete. Over the next days and weeks, the calcium silicates hydrate to form a calcium silicate hydrate (C–S–H) gel together with crystals of calcium hydroxide:

\mathrm{2(3CaO{\cdot}SiO_2) + 6H_2O \rightarrow 3CaO{\cdot}2SiO_2{\cdot}3H_2O + 3Ca(OH)_2}

The C–S–H gel binds everything together and gives concrete most of its strength. Hydration continues for months, which is why concrete is kept damp while it cures, and why its standard strength is measured after 28 days. The calcium hydroxide makes concrete strongly alkaline, which protects the steel reinforcement inside from rusting.

Tips for remembering

  • Limestone + clay, cooked to clinker: about 75% limestone (lime) and 25% clay (silica and alumina) are heated to about 1450 °C.
  • Gypsum is the brake: about 2–5% gypsum slows the flash setting of tricalcium aluminate.
  • Setting is hydration, not drying: cement hardens by reacting with water, so concrete even sets under water.